Discrimination medium and article to be discriminated
US7388627B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Oct 27, 2004 |
| Grant date | Jun 17, 2008 |
| Priority date | — |
| Expiry date | May 23, 2025 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/31504
- WIPO fieldOther consumer goods
- WIPO sectorOther fields
Abstract
A breakable seal can be discriminated more easily than the conventional one. The discrimination medium 100 has a cholesteric liquid crystal layer 104, a substrate layer 105, an adhesive layer 102, and a partial peeling layer 103. The discrimination medium 100 has an adhesion strength XA between the adhesive layer 102 and the partial peeling layer 103, an adhesion strength XB between the partial peeling layer 103 and the cholesteric liquid crystal layer 104, and an adhesion strength XC between the cholesteric liquid crystal layer 104 and the substrate layer 105. The relationships XA<XB and XA<XC are satisfied at areas 106, 108, and 110. The relationships XC<XA and XC<XB are satisfied at areas 107 and 109. In the above manner, when the discrimination medium 100 is peeled from the article 101, the discrimination medium 100 is separated into a discrimination medium 116 and a discrimination medium 117. For example, the above cholesteric liquid crystal layer is provided to a breakable seal, so that the breakable seal which allows confirmation of whether or not the discrimination medium is authentic before the breakable seal is broken and which allows confirmation of breakage of he breaka…
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.