Patent · US Expired

Lithium and vanadium oxide, a preparation method thereof and the use of same as an active electrode material

US7396614B2 · kind B2 · utility

9Cited by
1References
40Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 8, 2002
Grant dateJul 8, 2008
Priority date
Expiry dateNov 27, 2024

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P70/50
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A lithium and vanadium oxide is described having the formula Li1+xV3O8, wherein 0.1≦×≦0.25. The oxide has a monoclinic crystalline structure and comprises non-agglomerated grains in the form of monocrystalline pellets having a length L of between 1 and 100 μm, a width W such that 4<L/W<100, and a thickness t such that 4 L/t<100, with t<W, the elongation axis of the pellets being axis b of the monoclinic cell. The oxide may be prepared by mixing the Li and V precursors, without grinding or compression, heating said mixture to 565° C.-585° C. and de-agglomerating the product obtained. The oxide is suitable for use as an active material for the positive electrode of a lithium battery.