Patent · US Expired

Electroconductive powder and method for production thereof

US7407606B2 · kind B2 · utility

13Cited by
13References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 22, 2004
Grant dateAug 5, 2008
Priority date
Expiry dateSep 19, 2024

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC01P2006/40
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

A method for producing a titanium dioxide powder having a well electroconductive layer containing substantially no antimony, which comprises providing a titanium dioxide powder containing specific amounts or less of alkali metals, such as sodium and potassium, alkaline earth metals, such as magnesium and calcium, and metals having a valence of four or less, such as aluminum, zinc and iron, preparing an aqueous suspension of the titanium dioxide powder, adding an acidic aqueous solution containing a tin compound and a phosphorus compound and an alkaline solution to the above aqueous suspension so that the aqueous suspension has a pH in the range of 2 to 6 or 8 to 12, and firing the resulting product at a temperature of 600 to 925° C.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.