Patent · US Expired

Polymers of ethylene and, optionally, copolymerizable esters, films using such polymers and stretch hood packaging processes using such films

US7411026B2 · kind B2 · utility

5Cited by
7References
24Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 28, 2004
Grant dateAug 12, 2008
Priority date
Expiry dateJul 6, 2025

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/31938
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

Polymers comprising units derived from ethylene, said polymer having: a) a Melt Index of from 0.05 to 20 g/10 min. as determined by ASTM-1238 Condition E; b) at least 10 per 1000 C-atoms of short chain branches, containing five carbon atoms or less, as determined by C13 NMR, and less than 3.5 mol %, of units derived from a copolymerizable ethylenically unsaturated ester; c) a density of from 0.90 to 0.94 g/cm3, preferably 0.91 to 0.935 g/cm3, especially 0.92 to 0.93 g/cm3 as determined by ASTM D1505; and d) a relaxation time as described herein of at least 10 s. Such polymers can be obtained by free radical polymerization using a chain transfer agent that incorporates into the polymer chain such as an alpha-olefin, preferably propylene, as a chain transfer agent, preferably in a tubular reactor under circumstances to favor LCB formation in a down stream part of the tubular reactor.