Fiber board and its producing method
US7416779B2 · kind B2 · utility
Assignees
Inventors
Key dates
| Filing date | Sep 17, 2003 |
| Grant date | Aug 26, 2008 |
| Priority date | — |
| Expiry date | Sep 17, 2023 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/3179
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
To provide a fiberboard capable of reducing a load on the environment at all states of producing, using, and abolishing and moreover having a high degree of bending strength and a high bending-strength retention rate at high temperature and high humidity so as to be usable for an automobile interior material or building material and a fiber-board producing method. The fiberboard is formed by mixing natural fiber with polylactic acid resin serving as a binder and has an apparent density of 0.2 g/cm3.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.