Optical glass
US7419923B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jan 29, 2003 |
| Grant date | Sep 2, 2008 |
| Priority date | — |
| Expiry date | Dec 10, 2024 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S501/903
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
An optical glass comprising in mass %:The optical glass should preferably contain 0.1-5% WO3, 3.6-15% MgO, 0.1-5% Li2O+Na2O+K2O, 0—less than 0.5% and Sb2O3+As2O3 with the mass ratio of ZnO/BaO being 0.12—less than 0.50. The optical glass should preferably have refractive index (nd) within a range from 1.54 to 1.65 and Abbe number (νd) within a range exceeding 57 up to 69 and liquid phase temperature within a range from 870° C. to 930° C. There is provided an optical glass having high resistance to devitrification and medium refractive index and low dispersion characteristics which is free of ingredients such as Ta2O5 having a high cost of raw material and therefore can be manufactured at a relatively low cost of raw materials.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.