Abstract
A method of producing a non-metal element or a metal or an alloy thereof from a halide or mixtures thereof. The halide or mixtures thereof are contacted with a stream of liquid alkali metal or alkaline earth metal or mixtures thereof in sufficient quantity to convert the halide to the non-metal or the metal or alloy and to maintain the temperature of the reactants at a temperature lower than the lesser of the boiling point of the alkali or alkaline earth metal at atmospheric pressure or the sintering temperature of the produced non-metal or metal or alloy. A continuous method is disclosed, particularly applicable to titanium.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.