Patent · US Expired

Microporous polyethylene film and method of producing the same

US7435761B2 · kind B2 · utility

0Cited by
21References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 20, 2004
Grant dateOct 14, 2008
Priority date
Expiry dateMar 20, 2025

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

Disclosed is a microporous polyethylene film for a battery separator and a method of producing the same. The microporous polyethylene film comprises a resin mixture, which includes 100 parts by weight of composition containing 20-50 wt % polyethylene with a weight average molecular weight of 5×104-3×105 (component I) and 80-50 wt % diluent (component II), 0.1-2 parts by weight of peroxide (component III), and 0.05-0.5 parts by weight of anti-oxidant (component IV). The microporous polyethylene film has a puncture strength of 0.22 N/μm or more and a gas permeability (Darcy's permeability constant) of 1.3×10−5 Darcy or more. The present invention increases production efficiency of the microporous film, and improves performances and stability of the battery when the microporous polyethylene film is used in a battery separator.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.