Lead-free steel for machine structural use with excellent machinability and low strength anisotropy

US7445680B2 · kind B2 · utility

2Cited by
6References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 6, 2004
Grant dateNov 4, 2008
Priority date
Expiry dateDec 13, 2025

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C38/60
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A lead-free steel for machine structural use with excellent machinability and low strength an isotropy, which does not contain Pb and is equal to or higher than a conventional D Pb-containing free cutting steel in properties, is provided. This steel includes, on the weight basis, C: 0.10 to 0.65%; Si: 0.03 to 1.00%; Mn: 0.30 to 2.50%; S: 0.03 to 0.35%; Cr: 0.1 to 2.0%; Al: less than 0.010%; Ca: 0.0005 to 0.020%; Mg: 0.0003 to 0.020%; 0: less than 20 ppm; and the balance being Fe and inevitable impurities.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.