Patent · US Expired

Long fatigue life nitinol

US7455738B2 · kind B2 · utility

11Cited by
32References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 27, 2003
Grant dateNov 25, 2008
Priority date
Expiry dateNov 24, 2025

Classification

  • Technology area (CPC A)Human Necessities
  • CPC primaryA61L2400/16
  • WIPO fieldMedical technology
  • WIPO sectorInstruments

Abstract

A high fatigue life superelastic nickel-titanium (nitinol) wire, ribbon, sheet, tubing, or the like is disclosed. The nitinol has a 54.5 to 57.0 weight percent nickel with a balance of titanium composition and has less than 30 percent cold work as a final step after a full anneal and before shape setting heat treatment. Through a rotational beam fatigue test, fatigue life improvement of 37 percent has been observed.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.