Method for improving compression set in thermoplastic vulcanizates
US7504458B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Apr 12, 2006 |
| Grant date | Mar 17, 2009 |
| Priority date | — |
| Expiry date | Jan 17, 2027 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08L2312/00
- WIPO fieldMacromolecular chemistry, polymers
- WIPO sectorChemistry
Abstract
The compression set [(70° C., 22 hr), (100° C., 22 hr)] of TPVs can be improved by substituting, within their respective constituent plastic phase, all or portions of polyolefins having a high melting point, with polyolefins having lower melting point (Tm from between 115° C. to 140° C.). Exemplary polyolefins having melting points in this range include homopolyethylene, syndiotactic polypropylene, and isotactic poly(1-butene). Composition and methods of formulating thermoplastic vulcanizates to achieve an improved high temperature (between 70° C. 100° C.) compression set by selecting between suitable polyolefins on the basis of melting point temperature and substituting from 30% to 100% of high melting point polyolefins with low melting point polyolefins in the plastic phase are taught.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.