Optical resin film and polarizing film and liquid crystal display device using the same
US7532286B2 · kind B2 · utility
1Cited by
0References
8Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Aug 16, 2006 |
| Grant date | May 12, 2009 |
| Priority date | — |
| Expiry date | Nov 15, 2027 |
Classification
- Technology area (CPC G)Physics
- CPC primaryG02F2413/04
- WIPO fieldOptics
- WIPO sectorInstruments
Abstract
An optical resin film, which has Re (λ) and Rth (λ) satisfying retardation requirements (A) to (D), and has a thickness of from 30 μm to 80 μm: (A) 0.1<Re (450)/Re (550)<0.95 (B) 1.03<Re (650)/Re (550)<1.93 (C) 0.4<(Re/Rth (450))/(Re/Rth (550)))<0.95 (D) 1.05<(Re/Rth (650)/(Re/Rth (550))<1.9, and a polarizing plate and a liquid crystal display device using the optical resin film.