Patent · US Expired

Method of forming CMC component

US7550107B2 · kind B2 · utility

13Cited by
8References
17Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 25, 2005
Grant dateJun 23, 2009
Priority date
Expiry dateMay 18, 2026

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B2235/96
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method of forming a ceramic matrix composite (CMC) article (30) or a composite article (60) that minimizes the risk of delaminations while simultaneously maintaining a desired degree of porosity in the material. A pressure P applied against a surface of the article during a sintering process is controlled to be high enough to resist a separation force between the plies (66) of the CMC material (62) caused by anisotropic shrinkage of the material and/or to resist a separation force caused by differential shrinkage between the CMC material and an adjoined monolithic ceramic material (64). The pressure is also controlled to be low enough to avoid undue consolidation of the materials and to provide a desired degree of porosity in the sintered article. The pressure may be applied by delta-alpha tooling, and it may be varied verses the time of the sintering heating and/or across the article surface.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.