Patent · US Active

High surface area iron material prepared from a low surface area iron metal precursor

US7566680B2 · kind B2 · utility

1Cited by
25References
26Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 20, 2005
Grant dateJul 28, 2009
Priority date
Expiry dateJul 29, 2027

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB01J35/615
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

A method for producing a high surface area iron material starting with a low surface area iron metal is disclosed. The iron material of the present invention has a surface area of at least about 200 m2/g, and is prepared via a method which comprises reacting a low surface area iron metal with oxygen and an organic acid. The high surface area iron material formed via this method is essentially free of contaminants.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.