Metal stent with surface layer of noble metal oxide and method of fabrication
US7582112B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Dec 7, 2007 |
| Grant date | Sep 1, 2009 |
| Priority date | — |
| Expiry date | Dec 7, 2027 |
Classification
- Technology area (CPC A)Human Necessities
- CPC primaryA61F2310/00598
- WIPO fieldMedical technology
- WIPO sectorInstruments
Abstract
In a process for producing a biocompatible stent, a tubular substrate of the stent adapted for diametric expansion has a layer of a noble metal oxide formed over at least the outer surface of greater diameter of the substrate, the substrate being composed of a metal or an alloy thereof that is non-noble or less-noble than the layer's noble metal. An interface region adapted to prevent corrosion and to provide a firm bond between the surface of the substrate and the noble metal oxide layer is established, at least in part, by forming the noble metal oxide layer with a progressively varying concentration of noble metal-to-oxide with depth of the layer such that a surface of pure noble metal and negligible oxide of the layer is in closest proximity to the surface of the substrate. In one embodiment of the process, the interface region is established by forming the surface of pure noble metal and negligible oxide thereof in direct contact with the metal or alloy of the substrate surface. In another, the interface region is established by first creating an oxide of the substrate metal or alloy thereof at the substrate surface, and then forming the noble metal oxide layer as above, but i…
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.