Methods for reducing carbon contamination when melting highly reactive alloys
US7582133B2 · kind B2 · utility
14Cited by
7References
7Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Dec 27, 2006 |
| Grant date | Sep 1, 2009 |
| Priority date | — |
| Expiry date | Dec 27, 2026 |
Classification
- Technology area (CPC F)Mechanical Engineering; Lighting; Heating
- CPC primaryF27B14/10
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
Methods for reducing carbon contamination when melting highly reactive alloys involving providing a graphite crucible having an interior, applying at least a first protective layer to the interior of the graphite crucible, placing a highly reactive alloy into the crucible having the first protective layer, and melting the highly reactive alloy to obtain a melted alloy having reduced carbon contamination.