Treatment of hazardous waste material
US7585270B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Dec 5, 2007 |
| Grant date | Sep 8, 2009 |
| Priority date | — |
| Expiry date | Dec 5, 2027 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02W30/91
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method of incorporating a material in a settable binder is disclosed. The binder includes a source of caustic magnesium oxide. The method involves mixing the material with the binder, either as part of a slurry or for subsequent formation into a slurry, and then adding a setting agent to the slurry. The setting agent is added to enhance setting of the binder. The material can be a hazardous waste material or components thereof. The inventors have surprisingly discovered that when the setting agent is added after mixing of the material with the binder, that a superior setting of the material in the binder can be achieved. The settable composition can comprise only a caustic magnesium oxide binder and a setting agent for the binder, as the inventors have surprisingly discovered that there is no need for any other binding agents, thus providing a simpler binder composition and method of use.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.