Patent · US Active

Process for preparing a bituminous binder composition

US7592381B2 · kind B2 · utility

3Cited by
42References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 13, 2006
Grant dateSep 22, 2009
Priority date
Expiry dateSep 18, 2027

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08L53/02
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

The present invention is directed to a process for preparing a polymer modified bituminous binder composition in the substantial absence of crosslinking agents by heating a bitumen component in a stirred tank to a temperature from 185° C. to 221° C.; adding a block copolymer composition to the bitumen component while the bitumen component is being stirred to form a homogeneous mixture of the bitumen component and the block copolymer composition; and continuing to stir the homogeneous mixture while maintaining the temperature from 185° C. to 221° C. for a period of time from 4 hours to 30 hours thereby forming a cured polymer modified bituminous binder composition. The block copolymer composition utilized in the process comprises a diblock copolymer comprising one block of a monovinylaromatic hydrocarbon and one block of a conjugated diene having a peak molecular weight from 30,000 to 78,000 and a vinyl content from 35 to 80 mol percent based on the number of repeat monomer units in the conjugated diene block, and optionally one or more block copolymers comprising at least two blocks of monovinylaromatic hydrocarbon and at least one block of conjugated diene, the block copolymer sel…

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.