Producing nickel-base, cobalt-base, iron-base, iron-nickel-base, or iron-nickel-cobalt-base alloy articles by reduction of nonmetallic precursor compounds and melting
US7604680B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Mar 31, 2004 |
| Grant date | Oct 20, 2009 |
| Priority date | — |
| Expiry date | Aug 23, 2026 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P10/134
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A metallic article is produced by furnishing one or more nonmetallic precursor compound comprising the metallic base nickel, cobalt, iron, iron-nickel, or iron-nickel-cobalt, and at least one alloying element. The nonmetallic precursor compound(s) are chemically reduced to produce an initial metallic particle without melting the initial metallic particle. The initial metallic particle is thereafter melted and solidified to produce the metallic article. The melted-and-solidified metal may be used in the as-cast form, or it may be converted to billet and further worked to the final form.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.