Patent · US Active

Liquid-crystalline polymer composition, method for producing the same, and molded article using the same

US7618552B2 · kind B2 · utility

9Cited by
8References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 9, 2007
Grant dateNov 17, 2009
Priority date
Expiry dateOct 9, 2027

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC09K2323/02
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A liquid-crystalline polymer composition with less warpage not only in molding but also in a high temperature treatment conducted after molding is provided. The liquid-crystalline polymer comprises (i) 30 to 95% by weight of a first liquid-crystalline polymer having a deflection temperature under load of 200° C. or higher and (ii) 5 to 70% by weight of a second liquid-crystalline polymer having a deflection temperature under load lower than that of the first liquid-crystalline polymer, a melting point from 270° C. to lower than 400° C. and a flow-beginning temperature of 270° C. or higher.