Patent · US Active

Bituminous binder composition and process for preparing the same

US7622519B2 · kind B2 · utility

7Cited by
31References
41Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 29, 2008
Grant dateNov 24, 2009
Priority date
Expiry dateJun 9, 2028

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08L2555/84
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

The present invention is directed to a process for preparing a polymer modified bituminous binder composition in the substantial absence of crosslinking agents by heating a bitumen component in a stirred tank to a temperature from 160° C. to 221° C.; adding a block copolymer composition to the bitumen component while the bitumen component is being stirred to form a homogeneous mixture of the bitumen component and the block copolymer composition; and continuing to stir the homogeneous mixture while maintaining the temperature from 180° C. to 221° C. for a total period of time from 4 hours to 30 hours thereby forming a cured polymer modified bituminous binder composition. The block copolymer composition utilized in the process comprises one or more block copolymers having at least one monovinylaromatic block and either (I) at least one polybutadiene block having a vinyl content of less than 15 mol percent and at least one polybutadiene block having a vinyl content of greater than 25 mol percent or (II) at least one polybutadiene block having a vinyl content that tapers from a vinyl content of less than 15 mol percent at the first end adjacent to the monovinylaromatic block to a vinyl…

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.