Polymers of ethylene and, optionally, copolymerizable esters, films using such polymers and stretch hood packaging processes using such films
US7632573B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jul 3, 2008 |
| Grant date | Dec 15, 2009 |
| Priority date | — |
| Expiry date | Jul 3, 2028 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/31938
- WIPO fieldSurface technology, coating
- WIPO sectorChemistry
Abstract
The invention relates to a polymer comprising units derived from ethylene having: a) a Melt Index of from 0.05 to 20 g/10 min; b) at least 10 per 1000 C-atoms of short chain branches, containing five carbon atoms or less, and less than 3.5 mol %, of units derived from a copolymerizable ethylenically unsaturated ester, c) a density of from 0.90 to 0.94 g/cm3, preferably 0.91 to 0.935 g/cm3, especially 0.92 to 0.93 g/cm3, and d) a relaxation time as described herein of at least 10 s. The polymer may be used for stretch hood film, preferably as a blown film coextruded tube comprising: a) a core of the above polymer; and b) a skin layer, on each side of the core which may be of the same or different composition, comprising at least 60 wt % of an LLDPE having density of 0.91 to 0.94 g/cm3.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.