Patent · US Expired

Glass flake and method of manufacrturing the same

US7641730B2 · kind B2 · utility

3Cited by
7References
16Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 27, 2004
Grant dateJan 5, 2010
Priority date
Expiry dateMar 19, 2025

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/2996
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The present invention provides a glass flake having sufficiently high visible-light absorptivity. The glass flake of the present invention includes a glass composition that contains a transition metal oxide such as an iron oxide and that allows the glass flake to have a visible-light transmittance of 85% or lower measured with an A light source when the glass flake has a thickness of 15 μm. In this glass composition, it is preferable that the content of Fe2O3 (T−Fe2O3) in terms of the total iron satisfies the following formula, expressed in mass %: 10<T−Fe2O3≦50.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.