Si-C-O composite, making method, and non-aqueous electrolyte secondary cell negative electrode material
US7658863B2 · kind B2 · utility
23Cited by
10References
18Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Jul 21, 2005 |
| Grant date | Feb 9, 2010 |
| Priority date | — |
| Expiry date | Jun 17, 2027 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/2998
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
A Si—C—O composite powder is obtained by curing a reactive silane or siloxane having crosslinkable groups through heat curing or catalytic reaction into a crosslinked product and sintering the crosslinked product in an inert gas stream at a temperature of 700-1,400° C. into an inorganic state. It exhibits satisfactory cycle performance when used as the negative electrode material for non-aqueous electrolyte secondary cells.