Two-step method of coating an article for security printing by application of electric or magnetic field

US7674501B2 · kind B2 · utility

7Cited by
145References
9Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 1, 2006
Grant dateMar 9, 2010
Priority date
Expiry dateMar 23, 2028

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/25
  • WIPO fieldOther consumer goods
  • WIPO sectorOther fields

Abstract

A two-step method of making of a security printed image is disclosed and includes coating of the surface of a substrate with a predetermined image shape with an ink containing flaked magnetic pigment in a predetermined concentration, exposing a wet printed image to a magnetic field to align magnetic particles in a predetermined manner, allowing the ink to cure, and coating the substrate with a second printed image on the top of the first image. The second printed image with the same or different image shape is printed with another ink containing clear or dyed ink vehicle mixed with flaked magnetic pigment in a low concentration, exposed to the magnetic field of the same or different configuration as the first printed image and cured until the ink is dry.