Oxide ion conductor
US7682528B2 · kind B2 · utility
0Cited by
0References
8Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Sep 18, 2006 |
| Grant date | Mar 23, 2010 |
| Priority date | — |
| Expiry date | Aug 11, 2028 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P70/50
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
An La2O3 powder and an SiO2 powder are mixed with each other, and then heated. By heating, a porous material of LaXSi6O1.5X+12 (8≦X≦10) as a composite oxide is produced. Subsequently, the porous material is pulverized to obtain a powder, and the powder is added to a solvent to prepare a slurry. The slurry is solidified in a magnetic field to prepare a compact. After that, the compact is sintered, and an oxide ion conductor is obtained thereby.