Patent · US Active

Process for producing honeycomb structure

US7704442B2 · kind B2 · utility

6Cited by
4References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 12, 2008
Grant dateApr 27, 2010
Priority date
Expiry dateSep 12, 2028

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/24149
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

A process for producing a honeycomb structure by obtaining clay from a cordierite-forming raw material containing an alumina source, a silica source, and a magnesia source; and forming the clay into a honeycomb shape, wherein a material having, in its volume particle size distribution, a 50 volume % particle size (V50) [μm] of 1 to 25 μm is used, as each of alumina source, silica source, and magnesia source; and a material having, in the volume particle size distribution of the whole cordierite-forming raw material, a ratio of 90 volume % particle size (Vall90) [μm] to 10 volume % particle size (Vall10) [μm] [a volume particle size distribution ratio (Vall90/Vall10)] of 10 or less and a difference (Vall90−Vall10) between 90 volume % particle size (Vall90) [μm] and 10 volume % particle size (Vall10) [μm] of 25 μm or less is used, as the cordierite-forming raw material.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.