Abstract
A method of making a wrought aluminium-magnesium alloy rolled product, having a composition (in wt. %) of: 3.1<Mg<4.5; 0.4<Mn<0.85; 0.4<Zn<0.8; 0.06<Cu<0.35; 0.06<Cr<0.2; Fe<0.35; Si<0.2; Zr<0.05; Ti<0.3; impurities≦0.05 each up to a total of max. 0.15, and balance aluminium.