Method of synthesis of proton conducting materials
US7736547B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Mar 11, 2008 |
| Grant date | Jun 15, 2010 |
| Priority date | — |
| Expiry date | Apr 8, 2028 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P70/50
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
A method of producing a proton conducting material, comprising adding a pyrophosphate salt to a solvent to produce a dissolved pyrophosphate salt; adding an inorganic acid salt to a solvent to produce a dissolved inorganic acid salt; adding the dissolved inorganic acid salt to the dissolved pyrophosphate salt to produce a mixture; substantially evaporating the solvent from the mixture to produce a precipitate; and calcining the precipitate at a temperature of from about 400° C. to about 1200° C.