Synthetic rubber with narrow molecular weight distribution, a process for its preparation and a method of use

US7763703B2 · kind B2 · utility

0Cited by
11References
10Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 11, 2006
Grant dateJul 27, 2010
Priority date
Expiry dateAug 14, 2027

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08F8/50
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A novel process is used to prepare synthetic rubbers (B) which feature very narrow molecular weight distribution and a correspondingly low value for the polydispersity index. The preparation process encompasses the treatment of a synthetic rubber with ultrasound, where the resultant synthetic rubber (B) has a lower weight-average molecular weight (Mw) than the synthetic rubber (A) used. The resultant synthetic rubbers (B) have excellent suitability for processing via extruder processes or injection-moulding processes.