Patent · US Active

Reduced maximum reducibility temperature zirconium oxide and cerium oxide based composition, method for the production and use thereof as a catalyst

US7767617B2 · kind B2 · utility

7Cited by
8References
24Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 17, 2004
Grant dateAug 3, 2010
Priority date
Expiry dateAug 11, 2027

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02T10/12
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

A composition is based on zirconium oxide and cerium oxide with a proportion of zirconium oxide amounting to at least 50% by mass, having a maximum reducibility temperature of no more than 500° C. and a specific surface of at least 40 m2/g after 6 hours calcination at 500° C. in the form of a tetragonal phase. The composition can be used as a catalyst.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.