Patent · US Active

Cladding ingot to prevent hot-tearing

US7789124B2 · kind B2 · utility

7Cited by
5References
10Claims
0Family size

Assignee

Inventor

Key dates

Filing dateOct 5, 2009
Grant dateSep 7, 2010
Priority date
Expiry dateOct 5, 2029

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB22D11/116
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method of casting an ingot of a metal having a susceptibility to hot-tearing while avoiding such hot tearing. The method involves co-casting a cladding metal on a surface of a metal core ingot as the ingot is being cast in a DC casting procedure. The cladding layer preferably contacts the core ingot at a position on the ingot surface where the metal of the ingot is incompletely solid, e.g. at a temperature between its solidus temperature and liquidus temperatures. The metal of the core ingot and the metal of the cladding layer are the same and, if they contain grain refiners, the are present in an amount of 0.005% by weight of the metal or less.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.