Alloy for lithographic sheet
US7789978B2 · kind B2 · utility
Assignee
Inventor
Key dates
| Filing date | Sep 11, 2002 |
| Grant date | Sep 7, 2010 |
| Priority date | — |
| Expiry date | Aug 17, 2025 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB41N1/083
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
There is disclosed an Al alloy suitable for processing into a lithographic sheet, the alloy having a composition in wt %: Fe up to 0.4; Si up to 0.25; Ti up to 0.05; Cu up to 0.05; Zr up to 0.005; Cr up to 0.03; Ni up to 0.006; V up to 0.03; Zn up to 0.008 to 0.15; Mg up to 0.30; Mn up to 1.5. Unavoidable impurities up to 0.05 wt % total Al balance. The alloy allows production of the required surface for lithographic sheet over a wide range of process conditions.