Patent · US Active

Mixture for anode of improved adhesive strength and lithium secondary battery containing the same

US7799462B2 · kind B2 · utility

0Cited by
2References
1Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 24, 2006
Grant dateSep 21, 2010
Priority date
Expiry dateApr 30, 2028

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

Provided is an anode mix for a secondary battery comprising an anode active material, a conductive material and a binder, wherein the anode mix contains 0.01 to 1.0% by weight of alumina having an average particle diameter of less than 1000 nm, based on the total weight of the mix, and a lithium secondary battery comprising the same. Therefore, the present invention can achieve increases in anode active material-conductive material adhesion and anode active material-current collector adhesion which are exerted by a binder, and ultimately can improve lifespan characteristics or cycle characteristics of the battery.