Method for making hot strips of lightweight construction steel
US7806165B2 · kind B2 · utility
Assignees
Inventors
Key dates
| Filing date | Dec 22, 2004 |
| Grant date | Oct 5, 2010 |
| Priority date | — |
| Expiry date | Sep 21, 2026 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC21D8/0426
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
In a method for making hot strips, a workable lightweight construction steel is used which in particular can easily be deep-drawn cold and includes the main elements Si, Al and Mn, with high tensile strength and good TRIP and/or TWIP characteristics. The mass % are as follows for C 0.04 to <1.0, Al 0.05 to <4.0, SI 0.05 to ≦6.0; Mn 9.0 to ≦30.0, the remainder being iron with the common incidental steel elements. The melt is cast in a horizontal strip casting unit, close to the final dimensions at calm flow and without bending to form a pre-strip in the range between 6 and 15 mm, and subsequently is fed for further processing.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.