Pigment

US7811375B2 · kind B2 · utility

4Cited by
8References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 17, 2006
Grant dateOct 12, 2010
Priority date
Expiry dateJan 17, 2026

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/31993
  • WIPO fieldTextile and paper machines
  • WIPO sectorMechanical engineering

Abstract

A heated mixture comprising dehydroxylated kaolin and a high refractive index pigment is disclosed. When the dehydroxylated kaolin is metakaolin, the heated mixture has a GE brightness greater than 86% and a Hunter yellowness index of less than about 11. When the dehydroxylated kaolin is fully calcined kaolin, the heated mixture has a GE brightness greater than 89%. The heated mixture is advantageously used in decorative paper.Also disclosed are methods of using and making the decorative paper, and decorative laminates containing the decorative paper.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.