Monolithic refractory material having low expansibility, high strength, and crack extension resistance

US7833923B2 · kind B2 · utility

0Cited by
5References
5Claims
0Family size

Assignees

Inventors

Key dates

Filing dateFeb 21, 2008
Grant dateNov 16, 2010
Priority date
Expiry dateNov 29, 2028

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC04B2235/96
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A monolithic refractory material is provided by a method including the steps of kneading cordierite powder having a median diameter in a range of 10 to 50 μm, and having a sharp mountain-like particle size distribution in which the content of particles smaller than 10 μm is 1% or more to 36% or less, the content of particles ranging from 10 μm or more to 50 μm or less is 50% or more to 75% or less, and the content of particles of 51 μm or more is 1% or more to 14% or less, and a solvent including water and alumina sol or silica sol solution.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.