Patent · US Active

Method for the preparation of γLiV2O5

US7842273B2 · kind B2 · utility

0Cited by
3References
9Claims
0Family size

Assignees

Inventors

Key dates

Filing dateOct 18, 2005
Grant dateNov 30, 2010
Priority date
Expiry dateApr 30, 2027

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

The invention relates to the preparation of an optionally carbonaceous γ-LiV2O5 material.The process consists in preparing a composition formed of carbon and of precursors of Li and of V and in subjecting it to a heat treatment. The composition is prepared by bringing carbon, α-V2O5 and a Li precursor into contact in amounts such that the ratio of the [V2O5]/[Li] concentrations is between 0.95 and 1.05 and the carbon is in excess of at least 25% with respect to the stoichiometry. The heat treatment is carried out in two stages: a first stage at a temperature between 90° C. and 150° C. for a time of 1 to 12 hours and a second stage at a temperature between 420° C. and 500° C. for a time of between 10 min and 1 hour, under a nitrogen or argon atmosphere or under vacuum.Applications: positive electrode active material.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.