Patent · US Active

Electrode material containing mixture of polyvinyl alcohol of high degree of polymerization and polyvinyl pyrrolidone as binder and lithium secondary battery employed with the same

US7846583B2 · kind B2 · utility

7Cited by
3References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 24, 2007
Grant dateDec 7, 2010
Priority date
Expiry dateAug 24, 2027

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

An electrode mix comprising a mixture of a polyvinyl alcohol with polyvinyl pyrrolidone as a binder and a lithium secondary battery comprising the same are disclosed. The electrode mix and lithium secondary battery according to the present invention enable stable maintenance of adhesion between active materials and/or adhesion between the active material and current collector and reduction of volumetric changes of anode active materials during repeated charge/discharge cycles, through the use of a polymer having an improved elongation percentage while exhibiting very high adhesive strength, as a binder of an electrode mix. Therefore, the present invention enables production of a large-capacity lithium secondary battery particularly using a silicon- or tin-based anode active material.