PAEK powder, in particular for the use in a method for a layer-wise manufacturing of a three-dimensional object, as well as method for producing it
US7847057B2 · kind B2 · utility
44Cited by
1References
13Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Apr 3, 2008 |
| Grant date | Dec 7, 2010 |
| Priority date | — |
| Expiry date | Apr 3, 2028 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10T428/2982
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
By a temper treatment a polyaryletherketone powder is processed such that it is particularly suited for the use in a method for a layer-wise manufacturing of a three-dimensional object. To this effect the powder is tempered at a temperature that is at least 20° C. above the glass transition temperature for at least 30 minutes before it is used as building material.