High belite-containing sulfoaluminous clinker, method for the production and the use thereof for preparing hydraulic binders
US7850776B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jun 29, 2009 |
| Grant date | Dec 14, 2010 |
| Priority date | — |
| Expiry date | Jun 29, 2029 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02W30/91
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A sulphoaluminate clinker includes as a phasic formulation, compared with the total weight of clinker: 5 to 25% of a calcium aluminoferrite phase with a formulation corresponding to the general formula C2AXF(1−X), with X comprised between 0.2 and 0.8; 15 to 35% of a calcium sulphoaluminate phase yee' limit (C4A3$); 40 to 75% belite (C2S); from 0.01 to 10% of one or several minor phases selected from the group consisting of calcium sulphates, alkali sulphates, perovskite, calcium aluminates, gehlenite, free lime and periclase, and/or a vitreous phase, and additives including at least sodium and boron present in the following quantities, by weight as compared to the total weight of the clinker: from 0.1 to 5% of sodium expressed as sodium oxide and from 0.2 to 3% of boron, expressed as boron oxide, the total content of said additives being less than or equal to 15%.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.