Abstract
Before a thermally sprayed coating is deposited onto a cylindrical internal surface of a cylinder bore 3a rough surface 13 is formed to increase the adhesion of the thermally sprayed coating. After forming the rough surface is completed, an internal diameter measurement surface that is smoother than the rough surface is formed on an axial end section of the internal cylindrical surface. The internal diameter of the cylinder bore is measured at the internal diameter measurement surface with an internal diameter measuring instrument. An appropriate thickness for the thermally sprayed coating is determined based on the measurement result.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.