Methods and systems for coating and sealing inside piping systems
US7858149B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jan 4, 2007 |
| Grant date | Dec 28, 2010 |
| Priority date | — |
| Expiry date | Oct 29, 2029 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY10S118/13
- WIPO fieldMechanical elements
- WIPO sectorMechanical engineering
Abstract
Methods and systems for cleaning, coating and sealing leaks in existing pipes, in a single operation. A piping system can be cleaned in one pass by dry particulates forced and pulled by air throughout the piping system by a generator and a vacuum. Pipes can be protected from water corrosion, erosion and electrolysis, extending the life of pipes such as copper, steel, lead, brass, cast iron piping and composite materials. Coatings can be applied to pipes having diameters up to approximately 6″. Leak sealants of at least approximately 4 mils thick can cover insides of pipes, and can include novel mixtures of fillers and epoxy materials, and viscosity levels. A positive pressure can be maintained within the pipes during applications. Piping systems can be returned to service within approximately 96 hours.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.