Optical element and method of manufacturing the same
US7898715B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | May 14, 2009 |
| Grant date | Mar 1, 2011 |
| Priority date | — |
| Expiry date | May 14, 2029 |
Classification
- Technology area (CPC G)Physics
- CPC primaryG02B5/22
- WIPO fieldOptics
- WIPO sectorInstruments
Abstract
Ink having the optimum contact angle relative to a partition wall is selected for forming a pixel, based on the relationship with an inclination angle of the partition wall. The ink applied to the opening of the partition wall is dried to form the pixel such that an outer edge in contact with the partition wall has a thickness of at least 35% of the maximum height of the partition wall and a difference between the maximum thickness and the average thickness and a difference between the minimum thickness and the average thickness are not larger than 35% of the average thickness in an effective pixel area.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.