US7922889B2 · kind B2 · utility

4Cited by
5References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 10, 2006
Grant dateApr 12, 2011
Priority date
Expiry dateDec 4, 2027

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/12479
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

An anodic oxide film is formed on an aluminium or aluminium alloy work piece by forming an anodic oxide film on the work piece by AC electrolysis followed by subjecting the work piece to DC electrolysis. The AC anodizing step may be conducted at a voltage of 5 to 30V for 30 seconds to 10 minutes and the DC anodizing step may be conducted at a voltage of 5 to 30V for a period of 1 to 20 minutes. The anodic oxide coating is suitable for adhesive bonding of aluminium alloy work pieces.