A heat treatment method for a nickel-based superalloy, in particular for the production of single-crystal components or directionally solidified components having a chemical composition permits full solution annealing at a temperature T1, the method comprising: partially solution annealing in a controlled manner at a temperature T2<T1 in a first step so as to obtain 5-10% of undissolved γ′ phase in a residual eutectic; and performing a two-stage ageing treatment at respectively lower temperatures in a second step. As a function of the selected level of the partial solution annealing temperature, the proportion of the undissolved γ′ phase can be adjusted in a controlled way, and the tolerance with respect to the disorientation of small-angle grain boundaries/grain boundaries can be increased.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.