Patent · US Active

Extended-baking process for glass deposition tubes

US7946135B2 · kind B2 · utility

1Cited by
13References
19Claims
0Family size

Assignees

Inventors

Key dates

Filing dateJan 2, 2008
Grant dateMay 24, 2011
Priority date
Expiry dateOct 13, 2029

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P40/57
  • WIPO fieldOther special machines
  • WIPO sectorMechanical engineering

Abstract

Disclosed is a method of heat treating quartz glass deposition tubes at between 900° C. and 1200° C. for at least 115 hours. The resulting deposition tubes are useful in forming optical preforms that can yield optical fibers having reduced added loss.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.