Patent · US Active

Glass composition

US7960301B2 · kind B2 · utility

15Cited by
3References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 4, 2006
Grant dateJun 14, 2011
Priority date
Expiry dateDec 30, 2026

Classification

  • Technology area (CPC G)Physics
  • CPC primaryG02F1/1333
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A glass composition which is reduced in the amount of residual bubbles and is produced using smaller amounts of an environmentally unfriendly component such as arsenic oxide and antimony oxide. This glass composition comprises, in terms of mass %: 40-70% SiO2; 5-20% B2O3; 10-25% Al2O3; 0-10% MgO; 0-20% CaO; 0-20% SrO; 0-10% BaO; 0.001-0.5% Li2O; 0.01-0.5% Na2O; 0.002-0.5% K2O; and 0-1.0%, excluding 0%, Cl.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.