Patent · US Active

Resin film, production method thereof, polarizing plate and liquid crystal display device

US7976914B2 · kind B2 · utility

4Cited by
1References
7Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 15, 2007
Grant dateJul 12, 2011
Priority date
Expiry dateMay 11, 2030

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC09K2323/031
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

A resin film has a photoelastic coefficient of from 0 to 30×10−8 cm2/N; and Re satisfying the following formulae (1) to (4):20 nm<Re(548)<300 nm  Formula (1):0.5<Re(446)/Re(548)<1  Formula (2):1.0<Re(629)/Re(548)<2.0  Formula (3):0.1%≦[{Re(548) at 25° C., 10% RH−Re(548) at 25° C., 80% RH}/Re(548) at 25° C., 60% RH]≦20%,  Formula (4):wherein Re(λ) represents an in-plane retardation at a wavelength of λ.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.