Method for preparing an improved bitumen by addition of polyphosphoric acid and a cross-linkable polymer

US7985787B2 · kind B2 · utility

19Cited by
15References
6Claims
0Family size

Inventor

Key dates

Filing dateMay 31, 2007
Grant dateJul 26, 2011
Priority date
Expiry dateNov 9, 2027

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08L101/00
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

Methods are provided for preparing a bitumen product having improved properties for use in asphalt road paving. In a preferred embodiment, polyphosphoric acid is added to heated bitumen and stirred for a period of time. After addition of the polyphosphoric acid, one or more sulfur-crosslinkable elastomers and one or more sulfur donor coupling agents is added to the heated bitumen and mixed. The polyphosphoric acid, sulfur-crosslinkable elastomers and sulfur donor coupling agents may also be added to separate quantities of bitumen, and the bitumens may be combined prior to use to obtain a final bitumen product having the desired characteristics.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.